Polymer Property : CTE, linear, Parallel to Flow = 143 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 143 µm/m-°C

@Temperature 23.0 - 60.0 °C
79.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide P1000IX3 PA6, Impact Modified, Injection Molded
Staramide P1000IX3 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI020 or Star X 2020)Information provided by Eurostar.
CTE, linear, Parallel to Flow 143 µm/m-°C

@Temperature 23.0 - 60.0 °C
79.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermotuf P1000IX3 PA 6 (Europe-Africa-Middle East)
LNP* THERMOTUF* P1000IX3 is a compound based on PA6 resin containing Impact Modifier. Added features include : High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..