Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 132 µm/m-°C

@Temperature -30.0 - 30.0 °C
73.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP KL003LH Acetal
LNP* LUBRICOMP* KL003LH is an Acetal based compound containing 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant.
CTE, linear, Parallel to Flow 132 µm/m-°C

@Temperature 23.0 - 60.0 °C
73.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT (Europe-Africa-Middle East)
LNP* Lubricomp* WP004 is a compound based on Polybutylene Terephalate resin containing PTFE, Silicone. Added features include ; Internally Lubricated.
CTE, linear, Parallel to Flow 132 µm/m-°C
73.3 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® FG408L NC010 Nylon 66  (Unverified Data**)
Unreinforced Toughened Polyamide 66 with Developed for Food Contact Applications Zytel FG408L NC010 is a general purpose lubricated impact modified polyamide 66 resin with superior toughness for inj..