Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 111 µm/m-°C @Temperature 20.0 °C |
61.7 µin/in-°F @Temperature 68.0 °F |
|
Eastman Tenite 131E-28 Cellulose Acetate
(discontinued **) 28% plasticized and contains 50% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical. |
|||
CTE, linear, Parallel to Flow | 111 µm/m-°C @Temperature -40.0 - 40.0 °C |
61.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP KP004 Acetal LNP LUBRICOMP* KP004 is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 111 µm/m-°C @Temperature 23.0 - 60.0 °C |
61.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RL003 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RL003 is a compound based on Nylon 66 resin containing PTFE. |