Polymer Property : CTE, linear, Parallel to Flow = 107 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 107 µm/m-°C

@Temperature 20.0 °C
59.4 µin/in-°F

@Temperature 68.0 °F
Eastman Tenite 371A-10 Cellulose Acetate Propionate  (discontinued **)
10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
CTE, linear, Parallel to Flow 107 µm/m-°C

@Temperature -30.0 - 30.0 °C
59.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP KL003 Acetal Copolymer
LNP LUBRICOMP* KL003 is a compound based on Acetal Copolymer resin containing 15% PTFE. Added feature of this material is: Wear Resistant.
CTE, linear, Parallel to Flow 107 µm/m-°C

@Temperature 23.0 - 60.0 °C
59.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP MB006S PP (Europe-Africa-Middle East)
LNP* Thermocomp* MB006S is a compound based on Polypropylene resin containing Glass Bead. Added features of this material include: Heat Stabilized.
CTE, linear, Parallel to Flow 107 µm/m-°C

@Temperature 23.0 - 60.0 °C
59.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP MB006SXP PP (Europe-Africa-Middle East)
LNP* Thermocomp* MB006SXP is a compound based on Polypropylene resin containing Glass Bead. Added featurs include: Heat Stabilized.
CTE, linear, Parallel to Flow 107 µm/m-°C

@Temperature 20.0 °C
59.4 µin/in-°F

@Temperature 68.0 °F
Eastman Tenite 383A-12 CAP Cellulose Acetate Propionate  (discontinued **)
12% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.