Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Fusion | 46.0 J/g | 19.8 BTU/lb | Crystallization Heat; ASTM D3418 |
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Heat of Fusion | 46.0 J/g | 19.8 BTU/lb | ASTM D3418 |
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |