Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -6.67 °C | 20.0 °F | |
Greene Tweed FLUORAZ® 784 Fluoroelastomer, FEPM Sanitary gaskets made from Fluoraz® 784 work well in Sip and CIP applications where a low durometer elastomer compound is needed. While EPDMs and FKMs can provide a seal for extended periods, ch.. |
|||
Minimum Service Temperature, Air | -6.67 °C | 20.0 °F | |
Greene Tweed FLUORAZ® 790 Fluoroelastomer, FEPM Greene, Tweed`s Fluoraz® functions effortlessly in a variety of challenging process environments. Fluoraz performs well in aggressive chemicals where ultrapure materials are not required. Known f.. |
|||
Minimum Service Temperature, Air | -6.67 °C | 20.0 °F | |
Greene Tweed FLUORAZ® 799 Fluoroelastomer, FEPM Greene, Tweed`s Fluoraz® functions effortlessly in a variety of challenging process environments. Fluoraz performs well in aggressive chemicals where ultrapure materials are not required. Known f.. |
|||
Minimum Service Temperature, Air | -6.67 °C | 20.0 °F | Approx. Cold test |
Lubriplate 130-A Calcium Type Multi-Purpose Grease These water resistant calcium type greases are designed for plain bearings, cams, slides, and other light-duty applications where temperatures do not exceed 170°F. See special applications. Appli.. |
|||
Minimum Service Temperature, Air | -6.67 °C | 20.0 °F | Approx. Cold test |
Lubriplate 930-A Bentone Type Multi-Purpose Grease Formulated for higher temperature applications. They are shear stable, multi-purpose greases for both plain and anti-friction bearings. This series works well up to 375°F / 191°C and for short.. |
|||
Minimum Service Temperature, Air | -6.67 °C | 20.0 °F | Approx. Cold test |
Lubriplate X-Heavy G.S. Lithium Based Grease For Open Gearing Lithium-based open gear grease made for all types of open gears. Available in 4 formulas for a variety of conditions and temperatures. Gear Shield Extra Heavy is for adverse conditions.Applications:.. |
|||
Minimum Service Temperature, Air | -6.67 °C | 20.0 °F | |
ConocoPhillips 1 Milube® Grease 2100T NLGI No. 1 Description: Conoco Milube Grease is a high-quality, extreme-pressure lithium 12-hydroxy grease with heavy base oil developed for use in heavily loaded industrial heavy-duty bearings characteristic .. |
|||
Minimum Service Temperature, Air | -6.67 °C | 20.0 °F | |
Alcoa KAMA 1120 Prime AntiFog OPS, Sheet
(discontinued **) CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati.. |
|||
Minimum Service Temperature, Air | -6.67 °C | 20.0 °F | |
Alcoa KAMA 1200 Utility Clear OPS, Sheet
(discontinued **) CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati.. |
|||
Minimum Service Temperature, Air | -6.67 °C | 20.0 °F | |
BCC Products KRYTOX V-116 Mold Release Agent KRYTOX SPRAY V-116 is a dry, waxy mold release. It is an anti-sick and paintable. It is ideal for use in a broad variety of applications, such as plastic injection molding. Rigid, semi-rigid and fle.. |
|||
Minimum Service Temperature, Air | -6.67 °C | 20.0 °F | |
Alcoa KAMA 1100 Prime Clear OPS, Sheet
(discontinued **) CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati.. |