Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | 593 °C | 1100 °F | |
Lucas-Milhaupt Black Flux Silver Brazing Flux Black Flux is a water base paste consisting of potassium salts of boron and fluorine. It is recommended for use with torch, induction, furnace, resistance, and other heating methods.AdvantagesNo gri.. |
|||
Minimum Service Temperature, Air | 593 °C | 1100 °F | |
Lucas-Milhaupt Dry Flux Silver Brazing Flux Dry Flux is a premium quality brazing flux in powdered form consisting of a unique combination of borates and fluorides for use with torch, induction, furnace, resistance, dip and other heating meth.. |
|||
Minimum Service Temperature, Air | 593 °C | 1100 °F | |
Lucas-Milhaupt Ultra Flux Silver Brazing Flux Ultra Flux is a water base paste consisting of a unique combination of potassium salts of fluorine and boric acid. It is recommended for use with torch, induction, furnace, resistance, dip and other.. |
|||
Minimum Service Temperature, Air | 593 °C | 1100 °F | Lower limit of working range |
Heatbath/Park 10699 Class IV Salt Neutral Salt Basically the same as Uni-Hard, except that it is formulated per MIL-S-10699-B, Class 4Information provided by Heatbath Corporation - Park Metallurgical. |
|||
Minimum Service Temperature, Air | 593 °C | 1100 °F | Lower limit of working range |
Heatbath/Park Uni-Hard IR High Speed Hardening Salt Frequently used as a preheat for tool hardening or as a heating medium for continuous production hardening. Dragout is minimal because of high fluidity. Uni-Hard IR is water-soluble and non-hygros.. |
|||
Minimum Service Temperature, Air | 593 °C | 1100 °F | Lower limit of working range |
Heatbath/Park Uni-Hard IR Neutral Salt Frequently used as a preheat for tool hardening or as a heating medium for continuous production hardening. Dragout is minimal because of high fluidity. Uni-Hard IR is water-soluble and non-hygros.. |
|||
Minimum Service Temperature, Air | 593 °C | 1100 °F | Lower limit of working range |
Heatbath/Park Uni-Hard IR Quenching and Tempering Salt Frequently used as a preheat for tool hardening or as a heating medium for continuous production hardening. Dragout is minimal because of high fluidity. Uni-Hard IR is water-soluble and non-hygros.. |
|||
Minimum Service Temperature, Air | 593 °C | 1100 °F | Lower limit of working range |
Heatbath/Park Wire Annealing Quenching and Tempering Salt Chloride and carbonate mixture recommended. For annealing nonferrous materials or for heat treating steel where slight decarburization is not desirable. Wire Annealing Salt is extremely fluid, compl.. |
|||
Minimum Service Temperature, Air | 593 °C | 1100 °F | |
Lucas-Milhaupt Dispensable Flux Dispensable Flux is a water base consisting of a unique combination of potassium salts of fluorine and boric acid. It is recommended for use with torch, induction, furnace, resistance, dip and other.. |
|||
Minimum Service Temperature, Air | 593 °C | 1100 °F | Lower limit of working range |
Heatbath/Park Uni-Hard IR Steel Brazing Neutral Salt Used for brazing similarly to Nu-Sal. It is more stable than Nu-Sal in the higher temperature range.Information provided by Heatbath Corporation - Park Metallurgical. |
|||
Minimum Service Temperature, Air | 593 °C | 1100 °F | Lower limit of working range |
Heatbath/Park Wire Annealing Salt Neutral Salt Chloride and carbonate mixture recommended. For annealing nonferrous materials or for heat treating steel where slight decarburization is not desirable. Wire Annealing Salt is extremely fluid, compl.. |