Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
Nye Lubricants 5301 (SVLG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
Nye Lubricants 750A (IG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
Nye Lubricants UniFlor 8981R (899RP-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
Nye Lubricants UniFlor 8981SR (899S-1-RP) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Precision Polymer Engineering S60N Silicone Rubber Red Silicone Rubber, 56-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aircraft Materials Specification DTD5582A Gr.. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering S70N Silicone Rubber Silicone Rubber, 66-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aircraft Materials Specification DTD5582A Grade .. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering S80N Silicone Rubber Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aircraft Materials Specification DTD5582A Grade .. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
NextGen Adhesives G907-27 Structural Adhesive Description: NGAC G907-27 is a medium viscosity polyamide adhesive system utilized extensively in industrial and structural applications.Advantages and Applications: The NGAC G907-27 provides excell.. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
NextGen Adhesives G907-31 Epoxy Adhesive Description: NGAC G907-31 is a medium viscosity epoxy adhesive system utilized extensively in industrial and structural applications.Advantages and Applications: The NGAC G907-31 provides excellent .. |
|||
Minimum Service Temperature, Air | >= -65.0 °C | >= -85.0 °F | Low Temp Flex - Base Material, TR10 |
Parker Chomerics CHO-SEAL 1285R Reinforced Conductive Elastomer Seal These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at.. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Parker Chomerics CHO-SHIELD® 610 A/B Epoxy Conductive Coating Description: CHO-SHIELD® 610 A/B is a highly conductive, two-component silver-plated-copper filled epoxy coating for application to non-conductive plastic substrates, particularly those subject to .. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Resin Technology Group 310 Porous Fill, Slow Set Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 310 Porous Fill, Slow Set Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Resin Technology Group 388 Metals, Small Gap Fill Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 388 Metals, Small Gap Fill Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Resin Technology Group 390 Surface Insensitive Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 390 Surface Insensitive Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Resin Technology Group 395 Plastics, Large Gap Fill Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 395 Plastics, Large Gap Fill Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Brittleness Temperature |
DuPont Performance Polymers Hypalon® 45 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound
(d Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato.. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Resinlab® RC8038 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Resinlab® RC8040 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Resinlab® RC8048 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
Nye Lubricants UniFlor 8920U (491UV) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
Nye Lubricants UniFlor 8921M (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Humiseal 1C55 Silicone Conformal Coating Humiseal 1C55 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Continuous |
Lord Adhesives Circalokâ„¢ 6037 Epoxy Adhesive Circalokâ„¢ 6037 is an epoxy adhesive formulated for use by the semiconductor industry. An easy-to-spread thixotropic paste, it offers high heat transfer, low shrinkage, and a coefficient of ther.. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Trelleborg Emerson & Cuming Eccobond® TP 50 Two-Component Low Temperature Performance Silicone Adhesive Emerson & Cuming TP 50 Eccobond® Two-Component Low Temperature Performance Silicone AdhesiveFilled, RTV silicone rubber, paste adhesive. Room temperature cure. Very flexible. Color coded for ease o.. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Trelleborg Emerson & Cuming Stycast® 2651-40/23LV Two-Component General Purpose Encapsulant Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as .. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Tra-Con Tra-Bond 813J01 Silicone Encapsulant TRA-BOND 813J01 is a silicone adhesive system formulated to provide excellent thermal conductivity. This unique product bonds well to difficult substrates. Typical applications include encapsulation.. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
Nye Lubricants UniFlor 8920 (491) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Parker Chomerics CHO-SHIELD® 2001 Conductive Coating Electrically conductive coatings provide corrosion protection for enclosure flanges which mate with EMI shielding gaskets. They can also provide a corrosion resistant conductive surface coating on a.. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Parker Chomerics CHO-SHIELD® 2002 Conductive Coating Electrically conductive coatings provide corrosion protection for enclosure flanges which mate with EMI shielding gaskets. They can also provide a corrosion resistant conductive surface coating on a.. |