Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 105 Cyanoacrylate, for difficult rubbers PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 790 Cyanoacrylate, Surface insensitive PERMABOND® 790 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 940 Cyanoacrylate, low odor PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 791 Cyanoacrylate, Surface insensitive PERMABOND® 791 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 801 Cyanoacrylate, High Temperature PERMABOND® 801 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 910 Cyanoacrylate, Methyl grade PERMABOND® 910 is the original 100%-methyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. .. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT is an one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation prof.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond EP17HT-LO One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT-LO is a one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation pr.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond EP21TP-2 Two Component Polysulfide Epoxy Adhesive and Sealant Master Bond Polymer Adhesive EP21TP-2 is a two component polysulfide/epoxy based adhesive/sealant formulated to cure at room temperature or more rapidly at elevated temperatures, with a 100 to 100 m.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond EP30-3LO Highly versatile, two part epoxy system for bonding, coating, sealing and casting Master Bond EP30-3LO is a two component epoxy system featuring a combination of optical clarity and light transmission, good glass transition temperature (Tg), great chemical resistance along with p.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond EP45HTMED Epoxy Resists Radiation and Steam Sterilization Description: Master Bond Polymer System EP45HTMED is a two component heat cured epoxy system for high performance structural bonding, sealing, coating and casting. It is especially designed for the .. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond EP45HTND-2 Chemically Resistant, Non-Drip Epoxy Description: Master Bond EP45HTND-2 is a two component epoxy system for high performance bonding, sealing and coating. It is used for applications requiring solid temperature resistance and capable .. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond Supreme 45HT Toughened Heat Resistant Two Component Epoxy Adhesive Master Bond Polymer Supreme 45HT is a two component epoxy adhesive featuring an attractive balance of superior shear and peel strengths for high performance structural bonding and coating suitable f.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond UV15LV One Component, UV Curable Epoxy Based System Product Description: Master Bond UV15LV is a high strength, low viscosity, epoxy based UV curable system for bonding, sealing and coating. It has low viscosity and it is widely used in a variety of .. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond Supreme 33 High Temperature Resistant, Structural Adhesive Description: Master Bond Polymer System Supreme 33 is a unique, room temperature curing, toughened epoxy adhesive/sealant, offering high temperature resistance. This innovative system offers high bo.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond UV15X-2GT One Component, UV Curable Glob Top Compound Master Bond Polymer System UV15X-2GT is a one component, easily processable, UV curable glob top, featuring exceptional durability and chemical resistance. UV15X-2GT is a thixotropic paste that hand.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond UV15X-6MED-2 UV Curable Compound for Medical Applications Description: Master Bond Polymer System UV15X-6MED-2 is a newly developed one component clear, non-yellowing, UV curable urethane elastomer system possessing high flexibility and outstanding abrasio.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 941 Cyanoacrylate, low odor PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 943 Cyanoacrylate, low odor PERMABOND 943 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond Supreme 45HTQ Quartz Filled, Heat Resistant Epoxy Compound Master Bond Polymer Adhesive Supreme 45HTQ is a two component, toughened, quartz filled epoxy compound for high performance structural bonding and casting. It is suitable for applications where long.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond UV15-7SP4 Low Shrinkage, One Component, UV Curable System Master Bond Polymer System UV15-7SP4 is a one component, low viscosity UV system with flexibility. UV15-7SP4 has very little shrinkage when curing and has non-yellowing properties. It bonds well to .. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond UV15-7SP4DC One Component, Dual Cured, Flexible UV System Master Bond Polymer System UV15-7SP4DC is a one component, optically clear, dual cured flexible UV and/or heat curable polymer system with extended service capability of -80°F to +250°F. It cures .. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 947 Cyanoacrylate, low odor PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond UV15X-5 One Component High Viscosity UV Curable System Master Bond Polymer System UV15X-5 is one component, non-yellowing, UV curable urethane elastomer system possessing high flexibility and outstanding abrasion resistance. This high viscosity system c.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond UV15X-6NONMED-2 Abrasion Resistant UV Curable Compound Description: Master Bond Polymer System UV15X-6NONMED-2 is a newly developed one component clear, non-yellowing, UV curable urethane elastomer system possessing high flexibility and abrasion resista.. |