Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 4570XB025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)< Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1165 Fiberglass This data represents typical values for the production material. The data should not be .. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 19146R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1523 FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneAppearance: Black silicone gum and rubber on fiberglass clothT.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 30300R062 0.062" (1.57 mm) Uncured Silicone Rubber on Kodacel Carrier Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberCarrier: KodacelAppearance: Red silicone gum on polymer linersThis data represents typical values for the production mate.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 30570R015 0.015" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 32580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on PET Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on PET CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data s.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 51571R018 0.018" (0.457 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave: Polyethylene Appearance: Black silicone gum on fiberglass clothThis da.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 51586R015H 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production mat.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 55148R036 0.036" (0.914 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber This data r.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 55946C028 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 162 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 56141R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass Side 1: Uncured Silicone Rubber This data represents typical values for the production m.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 56146R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red si.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 56606R026 0.027" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production materia.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon CP-301C Bulk Compound This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon CP-375CR Silicone Rubber bulk compound |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon CP-493C Bulk Compound This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon CP-498W Bulk Compound This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon P30670R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Uncured Silicone Rubber Substrate: Style 1165 FiberglassAppearance: Red silicone gum on fiberglass with polymer release linersThis data represents typical values for the.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 41600R025 0.025" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 41940C020 0.015" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 48362X005 0.005" (0.127 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassProduct Use: Flexible hose/duct substrateAppearance: Gray silicone rubber on fiberglass fabricThis data represents t.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 51271R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneProduct Use: Flexible heater in.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 51976R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mat.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon R31961R019 0.019" (0.483 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon R34256R063 0.063" ((1.60 mm) Uncured/Cured Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Rubber LayerSide 2: Uncured Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, mate.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon R35366X020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 1: Cured Silicone Rubber Appearance: Gray gum on glass fiber fabricThis data represe.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 41580R025 0.025" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 45561R007 0.007"(0.178 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberAppearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not .. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon R37500G060 0.060" (1.52 mm) Uncured Fluorosilicone with Release PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Fluorosilicone Carrier: Release PETThis data represents typical values for the production material. The data should not be used to write,.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 44406X015 0.015" (0.381 mm) Platinum Cured Silicone/Peroxide Catalyzed Silicone Design/Construction:Side 1: Platinum Cured SiliconeSide 2: Peroxide Catalyzed SiliconeAppearance: Gray silicone gum on fiberglass clothThis data represents typical values for the production material.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon R37652R0055 0.0055" (0.140 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 2113 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. .. |