Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 230 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 230A (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 315A (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 374A (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 715 (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 723G (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 723TF (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 811-1 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
Parker Chomerics CHO-SHRINK® Heat Shrink EMI Shielding Conductive Heat Shrinking Shielding. CHO-SHRINK tubing is a heat shrinkable polyolefin tubing which provides effective EMI shielding for cables, connectors and cable/connector terminations. CHO-SHRI.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 706C (IG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
Permabond 931 Cyanoacrylate PERMABOND 931 is a low odor, nonfogging, nonfrosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | t<sub>g</sub> |
Ethylene Propylene Rubber (EPM, EPDM) Satisfactory compatibility with fireproof hydraulic fluids, ketones, hot and cold water, alkalis, and ozone/strong oxidizing chemicals. Unsatisfactory compatibility with most oils, gasoline, kerosen.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Continuous useful temperature. |
Momentive Performance Materials RTV8262 Red General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M 5491 PTFE Extruded Film Tape 3M™ PTFE Extruded Film Tape has a film backing with a silicone adhesive.Information provided by 3M |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | cured 14 days @ 50% RH |
3M AC-236 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | cured 14 days @ 50% RH |
3M AC-236 Class C-80 Aerospace Sealant 3M Aerospace Sealant AC-236 Class C are two-component, manganese dioxide cured, liquid polysulfide polymer systems providing excellent fuel tank and fuselage seals. They have outstanding resistance .. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | AMS-S-8802, cured 14 days @ 50% RH |
3M AC-251 Gray Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-251 Gray Class B are two-part, quick curing, polysulfide based canopy and windshield sealants. These products are formulated for sealing acrylic, glass, and polycarbonate air.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | cured 14 days @ 50% RH |
3M AC-350 Class B-6 Aerospace Sealant 3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | MIL-PRF-81733 |
3M AC-665 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-665 Class B are two-part, manganese-cured, chromate containing, corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corros.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | cured 14 days @ 50% RH |
3M AC-730 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M Scotch-Weld™ GM18 Gasket Maker Anaerobic Adhesive 3M™ Scotch-Weld™ Gasket Maker Anaerobic Adhesives are one-component anaerobic sealants formulated to replace pre-cut gaskets or used as form-in-place gaskets that cure at room temperature and seal.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M Scotch-Weld™ LO5 Low Odor Instant Adhesive 3M™ Scotch-Weld™ Low-Odor Instant Adhesives are formulated to have low volatility while maintaining bonding of a wide rage of materials. Low volatility means that these products are not only low o.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M Scotch-Weld™ MG05 PR Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M Scotch-Weld™ MG100 LO Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M Scotch-Weld™ RT40 Retaining Compound Anaerobic Adhesives 3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M 5490 PTFE Extruded Film Tape 3M™ PTFE Extruded Film Tape has a film backing with a silicone adhesive.Information provided by 3M |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M Scotch-Weld™ MG1500 PR Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M Scotch-Weld™ SI5 Surface Insensitive Instant Adhesive 3M™ Scotch-Weld™ Surface Insensitive Adhesives bond rough, porous, contaminated, and acidic substrates including wood, cardboard, veneer, fabric, cork, and leather. SI5 (formerly SB20) is a very l.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M Scotch-Weld™ GM15 Gasket Maker Anaerobic Adhesive 3M™ Scotch-Weld™ Gasket Maker Anaerobic Adhesives are one-component anaerobic sealants formulated to replace pre-cut gaskets or used as form-in-place gaskets that cure at room temperature and seal.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Intermittent |
3M Scotch-Weld™ RT300B Rubber-Toughened Instant Adhesive 3M™ Scotch-Weld™ Rubber Toughened Instant Adhesives are formulated with a unique elastomer that maximizes impact, vibration, peel, and thermal cycling resistance while providing tough flexible bon.. |