Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -268 - -200 °C | -450 - -328 °F | Average value: -215 °C Grade Count:19 |
Overview of materials for Polytetrafluoroethylene (PTFE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v.. |
|||
Minimum Service Temperature, Air | -268 - -20.0 °C | -450 - -4.00 °F | Average value: -171 °C Grade Count:29 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Garlock GYLON® 3500 PTFE Gasketing, Silica Filler PTFE with silica filler.Improved sealing performance over conventional PTFEUnique manufacturing process minimizes cold flow problems typical of skived and expanded PTFE sheetsExcellent bolt torque r.. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Garlock GYLON® 3502 PTFE Gasketing, Silica Filler, Oxygen Service PTFE with silica filler - Oxygen serviceImproved sealing performance over conventional PTFEUnique manufacturing process minimizes cold flow problems typical of skived and expanded PTFE sheetsExcelle.. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Garlock GYLON® 3510 PTFE Gasketing, Barium Sulfate Filler PTFE with barium sulfate filler.Improved sealing performance over conventional PTFEUnique manufacturing process minimizes cold flow problems typical of skived and expanded PTFE sheetsExcellent bolt .. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Garlock GYLON® 3535 PTFE Joint Sealant Pure PTFE is chemically inert, withstands a wide range of chemicalsConforms to FDA regulationsInformation provided by Garlock Rubber Technologies |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Garlock GYLON® 3540 Microcellular PTFE Gasketing Microcellular PTFE.Highly compressible PTFE seals under low bolt load- suitable for many non-metallic flangesCompressible material conforms to surface irregularities, especially on warped, pitted or.. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Garlock GYLON® 3565 ENVELON® PTFE Gasketing, Glass Microsphere Filled PTFE with aluminosilicate microsphere filler.Soft, deformable exterior conforms to surface irregularities; ideal for worn, warped or pitted flangesStable blue core improves cold flow resistanceLow b.. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Garlock GYLON® 3594 PTFE Gasketing, Glass Fiber Filled PTFE with glass fiber fillerInformation provided by Garlock Rubber Technologies |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Saint-Gobain Fluoroloy® A15 High Performance Seal Material Improved sealing at low pressure; Can be abrasive running against soft metals
Information provided by Saint-Gobain Performance Plastics. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Saint-Gobain Fluoroloy® A16 High Performance Seal Material General purpose material for heat and wear resistance; Recommended for dry and poorly lubricated applications; Particularly suitable for water and steam service
Information provided by Saint-Goba.. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Saint-Gobain Fluoroloy® A01 High Performance Seal Material Excellent for light dynamic and static service; Limited wear and heat resistance; Low gas permeability; Good cryogenic properties; Moderate to hard vacuum service; FDA approved.
Information provide.. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Saint-Gobain Fluoroloy® A08 High Performance Seal Material Superior heat and wear resistance; Recommended for moderate to high speed dynamic service running against soft metals; Non-abrasive
Information provided by Saint-Gobain Performance Plastics. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
W. L. Gore GORE™ 800 PTFE Universal Pipe Gasket (Style 800) 100% expanded PTFE, with multi-directional strength. Resistant to all media in the 0-14 pH range, except molten alkali metals and element fluorine, particularly at elevated temperatures and pressure.. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Garlock GYLON® 3505 PTFE Gasketing, Glass Microsphere Filled PTFE with aluminosilicate microspheres - NSF 61 approved (drinking water) - Oxygen serviceImproved sealing performance over conventional PTFEUnique manufacturing process minimizes cold flow problems.. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Saint-Gobain Fluoroloy® A30 High Performance PTFE/Glass Seal Material Excellent heat, wear, and chemical resistance; Good cryogenic properties; Can be abrasive running against soft metals at high surface speed; Excellent material for back-up rings
Information .. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Saint-Gobain Rulon® J Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of f.. |