Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Recommended |
Nye Lubricants 272 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Recommended |
Nye Lubricants 702A-EP (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Recommended |
Nye Lubricants UniFlor 8170U (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Recommended |
Nye Lubricants UniFlor 8172R (829RP) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Precision Polymer Engineering C70M Chloroprene Rubber Chloroprene Rubber, 66-75 °IRHD. Formulated to meet British Standard BS2752 grade C70.Applications: A versatile rubber with good compression set properties, giving moderate resistance to petroleum.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Precision Polymer Engineering N70H Nitrile Rubber Nitrile Butadiene Rubber (NBR), 65-75 °IRHD. High acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene.Applications: The high acrylonitrile content of this rubber increases resist.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering N90B Nitrile Rubber General purpose, Nitrile Rubber, 85-95 °IRHD. Copolymer of acrylonitrile and butadiene. ASTM & ISO designation = NBR. ASTM D2000 line call-out: M4CH910, A25, B14, EF31, EO15, EO35, F16.Applications.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering N90K Nitrile Rubber Peroxide cured Nitrile Rubber, 85-95 °IRHD. Copolymer of acrylonitrile and butadiene. ASTM designation = NBR. ISO designation = NBR. ASTM D2000/SAE J200 line call-out M7BG910, B14, EA14, EF11, EF21.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Q50Y Polyurethane Rubber Yellow/Green Polyurethane Rubber, 50-60 °IRHD. ASTM & ISO designation = AU.Applications: Good abrasion resistance and tensile strength, with fluid compatibility approaching that of NBR. Polyuretha.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Q65B Polyurethane Rubber Sulphur cured, Polyurethane Rubber, 55-65 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG621, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resist.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Q70B Polyurethane Rubber Peroxide cured, Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG714, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resis.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Q70W Polyurethane Rubber Peroxide cured, off-white Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG714, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abra.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Q70X Polyurethane Rubber Peroxide cured, self-lubricating, Polyurethane Rubber, 65-75 °IRHD. Compounded with graphite or molyb-d. To meet ASTM line call-out M5BG714, B14, EO14, EO34. Polyester-based urethane. ASTM & ISO d.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Q80Y Polyurethane Rubber Peroxide cured, yellow Polyurethane Rubber, 75-85 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG814, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasio.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Q90A Polyurethane Rubber Peroxide cured, blue Polyurethane Rubber, 85-95 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG910, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion .. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Freudenberg Simrit V115 Standard Fluoroelastomer Excellent resistance to petroleum products and solvents. Very good high-temperature performance. Fluorocarbon elastomers make up the most widely used seals in the semiconductor industry. Avoid polar.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Freudenberg Simrit V123 Standard Fluoroelastomer Excellent resistance to petroleum products and solvents. Very good high-temperature performance. Fluorocarbon elastomers make up the most widely used seals in the semiconductor industry. Avoid polar.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Retraction Temperature, TR10; ASTM D1329 |
Seals Eastern 7346 Extreme Low Temperature Service Rubber HNBR for cold temp (-50°C) and/or aqueous serviceInformation provided by Seals Eastern. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Low Temperature Flexibility |
Sylvin Technologies 50423 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg B419 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg B545 High Quality Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg B571 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg E850 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg Hypalon® H608 Chlorosulphonated Polyethylene PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing .. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg Hypalon® H630 Chlorosulphonated Polyethylene PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing .. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg Hypalon® H711 Chlorosulphonated Polyethylene PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing .. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg P650 Epichlorohydrin There are three types of epichlorohydrin:1. Homopolymers of epichlorohydrin. Designated CO.2. Chopolymers of epichlorohydrin and etylene oxide. Designated ECO.Terpolymers of epichlorohydrin, etylene.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg B870 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
ChevronTexaco Dura-Lith® NLGI 000 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
ChevronTexaco Dura-Lith® NLGI 00 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |