Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -140 °C
-220 °F
DSC
Adamas Adalon® 113 PTFE, 23/2% Carbon/Graphite Filled
Information provided by Adamas, HPM
Minimum Service Temperature, Air -140 °C
-220 °F
DSC
Adamas Adalon® 252 PTFE, 28% Glass Fiber
Information provided by Adamas, HPM
Minimum Service Temperature, Air -140 °C
-220 °F
DSC
Adamas Adalon® 805 PTFE, 40% Bronze
Information provided by Adamas, HPM
Minimum Service Temperature, Air -140 °C
-220 °F
DSC
Adamas Adalon® 703 PTFE, 15% Carbon Fiber
Information provided by Adamas, HPM
Minimum Service Temperature, Air -140 °C
-220 °F
DSC
Adamas Adalon® 704 PTFE, Long Carbon Fiber
Information provided by Adamas, HPM
Minimum Service Temperature, Air -140 °C
-220 °F
DSC
Adamas Adalon® 254 PTFE, 28% Glass Fiber
Information provided by Adamas, HPM