Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -60.0 - -30.0 °C | -76.0 - -22.0 °F | Average value: -48.2 °C Grade Count:241 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Minimum Service Temperature, Air | -65.0 - -30.0 °C | -85.0 - -22.0 °F | Average value: -52.0 °C Grade Count:48 |
Overview of materials for Thermoset Polyurethane, Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values .. |
|||
Minimum Service Temperature, Air | -40.0 - -30.0 °C | -40.0 - -22.0 °F | |
SMAC SMACWRAP® EX Damping Material, 0.12 mm SMACWRAP® concept is a smart and lightweight solution to embed into composite structures a very thin viscoelastic material. The SMACWRAP® will then bring damping to the composite structure wit.. |
|||
Minimum Service Temperature, Air | -40.0 - -30.0 °C | -40.0 - -22.0 °F | |
SMAC SMACWRAP® ST Damping Material, 0.10 mm SMACWRAP® concept is a smart and lightweight solution to embed into composite structures a very thin viscoelastic material. The SMACWRAP® will then bring damping to the composite structure wit.. |
|||
Minimum Service Temperature, Air | -40.0 - -30.0 °C | -40.0 - -22.0 °F | |
SMAC SMACWRAP® ST Damping Material, 0.20 mm SMACWRAP® concept is a smart and lightweight solution to embed into composite structures a very thin viscoelastic material. The SMACWRAP® will then bring damping to the composite structure wit.. |
|||
Minimum Service Temperature, Air | -40.0 - -30.0 °C | -40.0 - -22.0 °F | |
SMAC SMACWRAP® ST Damping Material, 0.60 mm SMACWRAP® concept is a smart and lightweight solution to embed into composite structures a very thin viscoelastic material. The SMACWRAP® will then bring damping to the composite structure wit.. |
|||
Minimum Service Temperature, Air | -40.0 - -30.0 °C | -40.0 - -22.0 °F | |
SMAC SMACWRAP® ST Damping Material, 1 mm SMACWRAP® concept is a smart and lightweight solution to embed into composite structures a very thin viscoelastic material. The SMACWRAP® will then bring damping to the composite structure wit.. |
|||
Minimum Service Temperature, Air | -40.0 - -30.0 °C | -40.0 - -22.0 °F | |
SMAC SMACWRAP® EX Damping Material, 0.20 mm SMACWRAP® concept is a smart and lightweight solution to embed into composite structures a very thin viscoelastic material. The SMACWRAP® will then bring damping to the composite structure without.. |