Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Murtfeldt Murlubric® [FS] Oil Modified Nylon 6 Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | Recommended |
Nye Lubricants 185D (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | Recommended |
Nye Lubricants 231L (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | Recommended |
Nye Lubricants 787K (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | impact conditions and heavy loads not considered (dry sample) |
Omnia Plastica Omniamid PA6 G - G - at 50% RH Cast nylon 6. The method of production of this polyamide (i.e. the polymerisation of the caprolactam directly in the mould) allows the production of stock shapes in larger than normal dimensions, su.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | impact conditions and heavy loads not considered (dry sample) |
Omnia Plastica Omniamid PA6 GHR - HR - at 50% RH Cast nylon 6 produced with the addition of graphite and a special lubricator which gives to this product better properties than natural PA6G. Whilst retaining the general features of OMNIAMID G it i.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | impact conditions and heavy loads not considered |
Omnia Plastica PE 300 - Polyethylene 300 Molecular weight 300,000 polyethylene similar to the type 500 with higher rigidity and lower resistance to continuous shocks. The applications are similar to those of PE 500, being more commonly spe.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Precision Polymer Engineering E60D Ethylene Propylene Rubber Sulphur cured, Ethylene Propylene Terpolymer, 56-65 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated in accordance with BS2494 Type ‘W’. Water Research Council (WRC) teste.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Precision Polymer Engineering Q70B Polyurethane Rubber Peroxide cured, Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG714, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resis.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Precision Polymer Engineering Q90A Polyurethane Rubber Peroxide cured, blue Polyurethane Rubber, 85-95 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG910, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion .. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering C90B Chloroprene Rubber Chloroprene Rubber, 86-95 °IRHD. To meet British Standard BS5176 line call-out M2BC907.Applications: A versatile rubber with good compression set properties, giving moderate resistance to petroleu.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Chlorosulfonated Polyethylene Rubber (CM, CSM) The chlorine (in CM) or chlorine and chlorosulfonyl (CSM) groups prevent the crystallization that occurs on unmodified polyethylene. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Greene Tweed CHEMRAZ® 504 Perfluoroelastomer Greene Tweeds Chemraz® 504, a 65 Shore A hardness perfluoroelastomer, provides an extremely broad range of chemical resistance and is perfect for services with low pressures and/or low temperatur.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Greene Tweed CHEMRAZ® 517 Perfluoroelastomer Greene Tweed’s Chemraz® 517, a perfluoroelastomer, is a white specialty compound, perfect for applications where contamination from carbon black must be prevented. Chemraz 517 has a Shore A.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | Gehman T100 |
Zeon Chemicals HyTemp® AR12 AR Super ACM Polyacrylate Elastomer Curesite is optimized for improved long-term heat and compression set resistance over traditional acrylates with good low-temperature properties. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | Gehman T100 |
Zeon Chemicals HyTemp® PV-04 AR Polyacrylate Elastomer HyTemp PV-04 contains one or more acrylic esters. This polymer is specific to the peroxide vulcanized cure system.Peroxide curable elastomer suitable for O-rings, seals, and gaskets. Also used for b.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Trelleborg Commercial Neoprene® C722 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Dow Corning MOLYKOTE® G 68 Semi-synthetic greaseInformation provided by Dow Corning |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Covestro Apec® 1697 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Dura-Bar 100-70-03 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Bond Laminates TEPEX® dynalite 108-FGAL290(1)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Bostik 6332 Quick Setup EVA Glue Stick Bostik 6332 Quick Setup EVA Glue StickShort open time and quick set up. Low viscosity. Easy to gun. Withstands elevated temperatures. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | Service |
3M FM04190N White Polyester Label Products 3M™ White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ Adhesive P1480, which .. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
3M 525 Polyurethane Construction Sealant 3M™ 500-Series Polyurethane Construction Sealant, Polyurethane Sealant and Polyurethane Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. The.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Trelleborg Commercial Neoprene® C500 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Radici Heraflex® P 55D 11 I HF 330 Modified Polypropylene Shore hardness: 55D (3s)Shiny surface, very flexible even at very low T°C (to -30°C), good resistance to weather conditions, very light and recyclableApplication examples: hiding hard, winter foot.. |