Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -19.0 °C | -2.20 °F | TR test, TR10 |
Daikin DAI-EL G-801 Fluoroelastomer Copolymer, Peroxide Curable Grade, 66% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Good low-temperature and elasticity characteristics.Information provided by Daikin Industries. |