Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | Recommended |
Nye Lubricants 350-SBG-2 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | Recommended |
Nye Lubricants 573H-40 (NT) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | Recommended |
Nye Lubricants UniFlor 8622R (851RP) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | Temperature at which stiffness does not exceed 70 Mpa |
Precision Polymer Engineering N80N Nitrile Rubber Nitrile Rubber, 76-85 °IRHD. Copolymer of acrylonitrile and butadiene. Meets Aerospace Specification DTD5595A Grade 80. ASTM designation = NBR. ISO designation = NBR.Applications: Sealing petroleum.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering P90B Polyacrylate Rubber Polyacrylic or Polyacrylate Rubber, 85-95 °IRHD. Copolymer of ethyl acrylate and vinyl ether. ASTM & ISO designation = ACM.Applications: Extensively used in automotive transmission systems. Superi.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G50S FFKM White Perfluoroelastomer Perlast® G50S FFKM is a White Perfluoroelastomer 50-55 °IRHD. It has excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and extr.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G60H Perfluoroelastomer Special, pure white compound with excellent high temperature properties and wide chemical resistance. Extremely low outgassing properties.Applications: For use in applications which require exposur.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G60S FFKM White Perfluoroelastomer Perlast ® G60S FFKM is a White Perfluoroelastomer 56-65 °IRHD. It has excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and ext.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G70H Perfluoroelastomer Special, pure white compound with high temperature properties and wide chemical resistance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing p.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G70K Perfluoroelastomer Special white compound with wide chemical resistance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Recommended f.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G70R Red Perfluoroelastomer Excellent chemical resistance, steam resistance and good mechanical properties. Color coded for identification.Applications: Specially developed for critical applications where good chemical resista.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G80A Perfluoroelastomer A black general purpose perfluoroelastomer compound with excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Do not use any P.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G80T Perfluoroelastomer A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require long-ter.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G81H Perfluoroelastomer Special, pure white compound with PTFE blended for improved dynamic performance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties. .. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G81T Perfluoroelastomer A special black perfluoroelastomer compound with PTFE blended for improved mechanical performance. Excellent steam resistance and mechanical properties. Extremely low outgassing properties. Applica.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G90S White Perfluoroelastomer Perlast ® G90S is a White Perfluoroelastomer 86-95 °IRHD with excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and formulated .. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering V70W Fluoroelastomer Compound Off-white Fluoroelastomer Rubber, 65-75 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out M2HK710, A1-10, B38, EF31, EO78, Z1,.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering V85C Fluoroelastomer Compound Green Fluoroelastomer Rubber, 80-90 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out:- MHK710, A1-10, B38, EF31, EO78, Z1, Z2,.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G71H Perfluoroelastomer Special, white compound, with PTFE blended for improved dynamic performance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties. Appl.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G74P Translucent Perfluoroelastomer A translucent beige compound with semi-crystalline perfluoropolymer nano-filler, specially developed to meet the demands of the semiconductor and bio-analytical industries. Compatible with fluorine .. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering V60L Fluoroelastomer Compound Special steam resistant, Fluoroelastomer Rubber, 55-65 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out: M2HK610, A1-10, B37, B38, EF31, EO78, F15.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Manifattura Cattaneo PVC U Polyvinyl Chloride Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Freudenberg Simrit V141 Standard Fluoroelastomer Excellent resistance to petroleum products and solvents. Very good high-temperature performance. Fluorocarbon elastomers make up the most widely used seals in the semiconductor industry. Avoid polar.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Trelleborg B700 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Trelleborg B800 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
ChevronTexaco Dura-Lith® NLGI 2 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
ChevronTexaco NLGI 2 Moly Grease EP FeaturesChevron Moly Greases EP are general purpose, extreme pressure (EP) greases. They are manufactured using highly refined selected base oils, a lithium-12-hydroxystearate thickener, 3% molybden.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | See Note 1. |
ChevronTexaco Thread Compound Texaco Thread Compound delivers value through:Ability to meet API requirements for high-pressure thread compounds.Galling prevention — Prevents galling in threaded connections. Joints are easier to.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | Application |
3M 7113 Repositionable Paper Label Material 3M™ Repositionable Paper Label Material 7113 and 7142 with 3M™ Adhesive 1000 offer unique, one-piece removability from many surfaces, including fragile papers, and can be repositioned repeatedly f.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
GEHR Plastics PVC-U Polyvinylchloride Polyvinyl chloride is a flame retardant material with an exceptional chemical resistance and also with lower stress cracking. PVC-U shows high mechanical strength, tensile strength and the continuou.. |