Polymer Property : Crystallization Temperature = 280 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 133 - 138 °C
271 - 280 °F
Peak; ASTM D3418
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)
Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: Batteries; Membran..
Crystallization Temperature 133 - 138 °C
271 - 280 °F
Peak, DSC; ASTM D3418
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Information provided by Solvay Specialty Polymers.