Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 125 - 131 °C | 257 - 268 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF) Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional .. |
|||
Crystallization Temperature | 125 - 130 °C | 257 - 266 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers Solef® 32008 Polyvinylidene Fluoride (PVDF) Solef® 32008 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional .. |
|||
Crystallization Temperature | 125 °C | 257 °F | Dow Method (DSC) |
Dow UNIVAL™ DMDC-6143 NT 7 High Density Polyethylene Resin (HDPE) Excellent parison melt strength / low sag Good extrudability / process-ability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDC-6143 NT 7 is a polymer with broad molecular weight distri.. |
|||
Crystallization Temperature | >= 125 °C | >= 257 °F | |
Addcomp ADD-VANCE® NU 489 Nucleation masterbatch, PP based Fields of application: Extruded and injection molded articles made from PP resins.Examples: Extruded PP sheets, films, tapes and blow molded and injection molded articles, such as garden furniture, .. |
|||
Crystallization Temperature | 125 - 131 °C | 257 - 268 °F | Peak, DSC; ASTM D3418 |
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Information provided by Solvay Specialty Polymers. |