Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 133 - 138 °C | 271 - 280 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF) Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: Batteries; Membran.. |
|||
Crystallization Temperature | 133 - 138 °C | 271 - 280 °F | Peak, DSC; ASTM D3418 |
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Information provided by Solvay Specialty Polymers. |