Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 130 - 170 °C | 266 - 338 °F | Average value: 150 °C Grade Count:3 |
Overview of materials for Thermoplastic Polyimide, Unfilled |
|||
Vicat Softening Point | 150 - 170 °C | 302 - 338 °F | Average value: 161 °C Grade Count:10 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |