Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 77.0 - 79.0 °C @Load 5.00 kg |
171 - 174 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RE 612 Rigid PVC, Extrusion Spiral pipes |
|||
Vicat Softening Point | 77.0 - 79.0 °C @Load 5.00 kg |
171 - 174 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RH 206/C Rigid PVC, Antishock Extrusion Medium antishock profiles |
|||
Vicat Softening Point | 77.0 - 79.0 °C @Load 5.00 kg |
171 - 174 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RK 316 Rigid PVC, Extrusion Lead Free Indoor profiles |
|||
Vicat Softening Point | 77.0 - 79.0 °C @Load 5.00 kg |
171 - 174 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RKI 0223 Rigid PVC, Antishock Injection Molding Lead Free Fittings for building trade |
|||
Vicat Softening Point | 77.0 - 79.0 °C @Load 5.00 kg |
171 - 174 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RKI 0822 Rigid PVC, Antishock Injection Molding Lead Free Technical items |
|||
Vicat Softening Point | 77.0 - 79.0 °C @Load 5.00 kg |
171 - 174 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RKT 226 Rigid PVC, Extrusion Lead Free Metal effect profiles |
|||
Vicat Softening Point | 56.0 - 79.0 °C | 133 - 174 °F | Average value: 70.1 °C Grade Count:27 |
Overview of materials for Ionomer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Vicat Softening Point | 77.0 - 79.0 °C @Load 5.00 kg |
171 - 174 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RI 52/S Rigid PVC, Injection Molding Fittings for building trade |