Polymer Property : Vicat Softening Point = 369.7 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 187.6 °C
369.7 °F
10 N; ASTM D1525
CRP Technology Windform® FX Polyamide Composite
Processed by selective laser sintering (SLS). Windform® FX is a new generation polyamide based material, whose repeatability and mechanical characteristics make it particularly suited for Additive..