Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 107 °C | 225 °F | ASTM D-1525 |
Plaskolite West Optix® CP - 71 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Vicat Softening Point | 107 °C | 225 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® CX3222ME PC+ABS Cycoloy* resin grade CX3222ME is an extrudable & thermoformable PC/ABS blend with non brominated and non chlorinated flame retardant systems. Key features of low gloss and good impact make it ideal .. |
|||
Vicat Softening Point | 107 °C | 225 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics GELOY XP4034 ASA+PC (Europe-Africa-Middle East) GELOY XP4034 is a high heat modified ASA+PC alloy. It is a weatherable, injection mouldable product which is available in a wide range of colours. The product is recommended for automotive unpainted.. |
|||
Vicat Softening Point | 107 °C | 225 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® DMX9254 PC (Europe-Africa-Middle East) Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Vicat Softening Point | 107 °C | 225 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 8% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Vicat Softening Point | 107 °C | 225 °F | ASTM D1525 |
I. Stern WC-102 General Purpose Crystal Polystyrene Features:Good Processing CharacteristicsUL Classification 94 HBExcellent Water ClarityComplies with FDA Title 21 CFR 177.1640ApplicationsExtrusion FoamDisplaysInformation provided by I. Stern & Co. .. |
|||
Vicat Softening Point | 107 °C @Load 5.00 kg |
225 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical XR419 ABS, Heat Resistance, Chemical Resistance Feature: Injection Molding, Heat Resistance, Chemical ResistanceApplication: Automotives Interior Housing (Ventgrille Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provide.. |
|||
Vicat Softening Point | 107 °C @Load 1.00 kg, Thickness 3.17 mm |
225 °F @Load 2.20 lb, Thickness 0.125 in |
ASTM D1525 |
IRPC Polimaxx Polene GP110 Polystyrene APPLICATIONS: EXTRUSION SHEET, HOUSEHOLD PRODUCTS VACUUM SHEET , FOOD PACKAGING, TOY, SANITARY WARE, etc. |
|||
Vicat Softening Point | 107 °C | 225 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance. |
|||
Vicat Softening Point | 107 °C | 225 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® EF-1032 PC/ABS, Unreinforced FR Extrusion resin, non-halogen flame-retardantInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 107 °C | 225 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® EF-1032 PC/ABS, Unreinforced FR Extrusion resin, non-halogen flame-retardantInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 107 °C | 225 °F | |
Styron Magnum™ 275 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Vicat Softening Point | 107 °C | 225 °F | |
Styron Magnum™ 541 ABS, High Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Vicat Softening Point | 107 °C | 225 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL N190X PPE+HIPS (Asia Pacific) PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. Dielectric strength. Suitable for E/E market applications. |
|||
Vicat Softening Point | 107 °C | 225 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Asia Pacific) PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
Vicat Softening Point | 107 °C | 225 °F | B/120; ISO R306 |
Samsung Cheil Industries Starex® GR-4020L ABS, Glass Filled ABS/GF material that is used in printer LBP fuserInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 107 °C | 225 °F | A (10N); ISO 306 |
Borealis Himod™ FT7324 . LDPE for Film Himod FT7324 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |
|||
Vicat Softening Point | 107 °C | 225 °F | ASTM D1525 |
Eastman Tenite 360A4861307 Cellulose Acetate Propionate, Clear, Trsp Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAEase of processingGamma and.. |
|||
Vicat Softening Point | 107 °C | 225 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D1525 |
Eastman Tenite Propionate 383A2R30007 Natural, Trsp Cellulose Acetate Propionate Plasticizer 7%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Vicat Softening Point | 107 °C | 225 °F | ASTM D1525, ISO 306 |
DuPont™ Bynel® 50E739 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Vicat Softening Point | 107 °C | 225 °F | |
Dow Retain® ABS 7490 ABS Data provided by Dow Chemical. |
|||
Vicat Softening Point | 107 °C | 225 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D1525 |
Eastman Tenite Propionate 360E0096907 Natural, Trsp Cellulose Acetate Propionate Plasticizer 7%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.TENITE cellulosic plastics are noted for their excellent balance of properties - toughness, .. |
|||
Vicat Softening Point | 107 °C @Load 1.00 kg, Thickness 3.17 mm |
225 °F @Load 2.20 lb, Thickness 0.125 in |
ASTM D1525 |
Diamond Polymers ASAPC TA-45 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Vicat Softening Point | 107 °C @Load 0.999 kg |
225 °F @Load 2.20 lb |
ISO 306 |
Arkema Group OREVAC® 18350P Grafted Maleic Anhydride Polyethylene OREVAC 18350P is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE and HDPE coating for steel pipeline. It is mainly used in pipe coating to have good adhesion pe.. |
|||
Vicat Softening Point | 107 °C | 225 °F | ISO 306A |
Ineos Nova 201 Crystal Polystyrene High Heat Extrusion Grade
(discontinued **) Excellent heat resistance, Superior melt strengthApplications: Foam insulation, Oriented polystyrene sheet (OPS), XPS food packaging, Sheet and profile extrusionProperties were determined on injecti.. |
|||
Vicat Softening Point | 107 °C | 225 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
Vicat Softening Point | 107 °C | 225 °F | 50°C/hr; 50N |
Arkema Group Oroglas® V 825 T Acrylic
(discontinued **) OROGLAS V 825 T exhibits an excellent balance of properties including superior thermal resistance with an easy processing behavior.OROGLAS V 825 T is then the material of choice for automotive appli.. |
|||
Vicat Softening Point | 107 °C @Load 5.00 kg |
225 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical XR404T ABS, Heat Resistance Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9, and 9001-96-2Information provided by LG Chemical.. |
|||
Vicat Softening Point | 107 °C | 225 °F | |
Styron Magnum™ 9100 MFD ABS Data provided by Dow Chemical.This product line was spun off from Dow Chemical to Styron in 2010. |
|||
Vicat Softening Point | 107 °C | 225 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CP8320 PC+ABS (Asia Pacific) Cycoloy Medium Heat Plating Grade for Automotive |