Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 80.0 - 92.0 °C | 176 - 198 °F | Average value: 86.3 °C Grade Count:4 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |