Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 157 - 205 °C | 315 - 401 °F | Average value: 178 °C Grade Count:27 |
Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |
|||
Vicat Softening Point | 170 - 205 °C | 338 - 401 °F | Average value: 186 °C Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Vicat Softening Point | 79.0 - 205 °C | 174 - 401 °F | Average value: 126 °C Grade Count:44 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |