Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 107 - 160 °C | 225 - 320 °F | Average value: 130 °C Grade Count:6 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
Vicat Softening Point | 140 - 160 °C | 284 - 320 °F | Average value: 147 °C Grade Count:3 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Vicat Softening Point | 140 - 160 °C | 284 - 320 °F | Average value: 150 °C Grade Count:16 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
Vicat Softening Point | 145 - 160 °C | 293 - 320 °F | Average value: 157 °C Grade Count:31 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Vicat Softening Point | 53.0 - 160 °C | 127 - 320 °F | Average value: 113 °C Grade Count:112 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Vicat Softening Point | 140 - 160 °C | 284 - 320 °F | Average value: 154 °C Grade Count:11 |
Overview of materials for Nylon 11, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Vicat Softening Point | 130 - 160 °C | 266 - 320 °F | Average value: 148 °C Grade Count:20 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Vicat Softening Point | 90.0 - 160 °C | 194 - 320 °F | Average value: 151 °C Grade Count:19 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Vicat Softening Point | 108 - 160 °C | 226 - 320 °F | Average value: 128 °C Grade Count:9 |
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend". Each property range of values reported is minimum and ma.. |
|||
Vicat Softening Point | 55.0 - 160 °C | 131 - 320 °F | Average value: 111 °C Grade Count:6 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |