Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 47.2 °C | 117 °F | ASTM D1525 |
ExxonMobil OPTEMA™ TC 120 ExCo Ethylene Methyl Acrylate Product Description: Optema TC 120 is an ethylene methyl acrylate copolymer intended for extrusion coating, coextrusion coating and extrusion lamination where good interlayer adhesion between polyet.. |
|||
Vicat Softening Point | 47.2 °C | 117 °F | ASTM D1525 |
ExxonMobil Escorene® UL 7520 Adhesive Application Resin Escorene Ultra UL 7520 is a high flow, 18.5% vinyl acetate copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesives, sealan.. |