Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 42.2 °C | 108 °F | ASTM D1525 |
Dow Primacor® 5986 Ethylene acrylic acid copolymer Low heat seal temperature High gloss, excellent clarity Excellent grease and oil resistance and excellent product resistance for flexible packaging applications Complies with U.S. FDA 21 CFR 177.131.. |