Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 104R PC (Asia Pacific) LEXAN 104R is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information a.. |
|||
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 121 PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small intricate parts. |
|||
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 124R PC (Asia Pacific) LEXAN 124R is a low viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information an.. |
|||
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 131 PC Nonhalogenated. 3.5 MFR. |
|||
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 203 PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. |
|||
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® 223 PC 17.5 MFR, for small, intricate parts. Improved flame retardance. UV stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 244R PC (Asia Pacific) LEXAN 244R resin grade is a medium viscosity multi purpose product with improved flame resistance and release properties. It is also FDA food contact compliant available in limited colors. |
|||
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 500R PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. Internal mold release. |
|||
Vicat Softening Point | 154 °C | 310 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-BR1-UV Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilized Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilizedFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical.. |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Ravago Manufacturing Americas Hylex® P1007L Polycarbonate Information provided by Ravago |
|||
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® FXD103R PC (Asia Pacific) FXD103R is a Light Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect propert.. |
|||
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® FXD104R PC FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties. |
|||
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® FXE121R PC Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). MFR 18.2. Internal mold release. |
|||
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® FXE144H PC FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe.. |
|||
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® LUX2114G PC (Asia Pacific) 18 MFR. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® LUX2614 PC (Asia Pacific) 7.0 MFR. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® 134 PC (Asia Pacific) 3.5 MFR. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information and should not be used for medical applicati.. |
|||
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 141 PC General purpose polycarbonate with melt flow rate of 10.5. |
|||
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® 303 PC (Asia Pacific) Clear, high viscosity material designed to service severe environments of HID lighting.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® FXM141R PC (Asia Pacific) FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color .. |
|||
Vicat Softening Point | 154 °C | 309 °F | ASTM D1525-97 |
Ipiranga Petrochem PH 0241 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Vicat Softening Point | 154 °C | 309 °F | ASTM D1525 |
Shuman SP920 Black Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self-extinguishing.Data provided by the manufacturer. |
|||
Vicat Softening Point | 154 °C | 309 °F | |
Styron CALIBRE™ 701 15 Polycarbonate, General Purpose CALIBRE® 701 series polycarbonate resins are a general purpose, transparent, ignition resistant grades equipped with a mold release package. The CALIBRE 701 series resins exhibit a high heat resi.. |
|||
Vicat Softening Point | 154 °C @Load 1.02 kg |
309 °F @Load 2.25 lb |
A50; ISO 306 |
Borealis Borpact™ BC914TF Polypropylene Copolymer Borpact™ BC914TF is a high crystalline heterophasic copolymer film resin, based on special Borstar® nucleating technology. This grade is especially developed for the manufacturing of unoriented f.. |
|||
Vicat Softening Point | 154 °C @Load 1.02 kg |
309 °F @Load 2.25 lb |
ASTM D1525 |
Carmel Olefins CAPILENE® M 45 F Polypropylene Homopolymer CAPILENE® M 45 F is a polypropylene homopolymer developed for the production of cast films. It is formulated with slip and anti-blocking agents. They show high gloss, high transparency and good sti.. |
|||
Vicat Softening Point | 154 °C | 309 °F | 10 N; ASTM D1525 |
Braskem H 603 Blow Molding Polypropylene Description: H 603 is a low melt flow rate homopolymer used for general purposes. This resin is designed for blow moulding and extrusion applications. H 603 exhibits excellent processability, excell.. |
|||
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 243R PC 10.5 MFR. UV-stabilized. Improved flame retardance. Internal mold release. |
|||
Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® SFX123RU PC SFX123RU is a transparent SecurFX grade with improved flow, mold release and UV stabilizer. This grade is for security applications and contains proprietary authentication technology.This data was s.. |