Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 127 °C | 261 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Asia Pacific) UV stabilized, non-FR PC/ABS of excellent flow and impact performance |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS High impact PC+ABS material designed for local Pacific Automotive applications |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Asia Pacific) High impact PC+ABS material designed for local Pacific Automotive applications |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Europe-Africa-Middle East) High impact PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS (Europe-Africa-Middle East) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Eur.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS (Europe-Africa-Middle East) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Eur.. |
|||
Vicat Softening Point | 127 °C @Load 5.001 kg |
261 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH GF4030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Vicat Softening Point | 127 °C | 261 °F | 50°C/hr; 50N |
Polimeri Europa KOBLEND PCA 839F PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABSUnfilled. Suitable for Injection Molding. Supplied as pellets.ISO data. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses... |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
Chevron Phillips HiD® 9720 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear homopolymerCharacteristics: good flow, moderate impact strength, excellent stiffness, moderate ESCR, moderate shrinkage resistanceApplications: pails, structural foamInformation p.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ISO 306 |
Total Finathene® 53140 HDPE, blow molding, sheet
(discontinued **) Finathene® 53140 is a high density polyethylene produced by the slurry loop low pressure polymerization process FINATHENE® 53140 has been especially developed for the manufacturing of blow molded .. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
LyondellBasell Alathon® M5370PX High Density Polyethylene, Extrusion Grade ALATHON M5370PX is a copolymer with a narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processability. T.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
Global J-2308 High Density Polyethylene Description-industrial injection grade w/ UV stabilizer, good for high impact
strengthApplications-high quality industrial products, outdoor applications such as pallets & cratesInformation provided.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Europe-Africa-Middle East) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
Shuman 211 Flame Retardant Polyphenylene Ether Copolymer Alloy Black, Custom Colors. Excellent flame retardancy, easy processability, good impact strength, good chemical resistance, injection molding and extrusion grades.Data provided by the manufacturer. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS (Europe-Africa-Middle East) NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
A. Schulman LP479-01 High-Density Polyethylene Homopolymer DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
ExxonMobil HDPE HD 9830.02 High Density Polyethylene Resin Product Description: HD 9830.02 is a blow molding grade high density polyethylene copolymer with a bimodal molecular weight distribution. It provides a very good balance of stress crack resistance, .. |
|||
Vicat Softening Point | 127 °C | 260 °F | ASTM D1525 |
ExxonMobil Paxon™ AL55-003 Blow Molding Resin Product Description: AL55-003 is a blow molding grade high density polyethylene offering a good combination of stiffness and stress crack resistance.Availability: Latin America, North America and So.. |
|||
Vicat Softening Point | 127 °C @Load 1.00 kg |
261 °F @Load 2.20 lb |
ASTM D1525 |
Diamond Polymers ABS TS15v04 Injection Molding Grade, ABS/PC Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Vicat Softening Point | 127 °C | 261 °F | |
Dow DOWLEX™ IP-10262 High Density Polyethylene DOWLEX® IP-10262 resin is an improved processing high density polyethylene resin with controlled molecular weight distribution for use in reusable case applications including, poultry, fast food, a.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
Dow UNIVAL™ DMDA-6230 NT 7 High Density Polyethylene Resin (HDPE) Good extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6230 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipment to.. |
|||
Vicat Softening Point | 127 °C @Load 1.02 kg |
261 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem AC59 HDPE Monofilament Polyethylene Homopolymer AC59 resin is a high-density polyethylene homopolymer produced by the solution process and designed for monofilament applications. It contains antioxidant additives. Its applications include: film .. |
|||
Vicat Softening Point | 127 °C | 261 °F | 50°C/hr; 50N |
Arkema Group Pebax® MX 1059 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) Hardness 35 shore D Good resistance to oils. Applications: Automotive, cable...ISO data provided by the manufacturer, Arkema. |
|||
Vicat Softening Point | 127 °C | 261 °F | 10 N; ASTM D1525 |
Braskem Green PE SHD7255LSL Injection Molding High Density Polyethylene Description: SHC7260LS-L is a high-density polyethylene, developed for the injection molding which presents high hardness and stiffness, besides low tendency to warpage. This resin has additives aga.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
C.O.I.M. LARIPUR® LPR5225 Special Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Vicat Softening Point | 127 °C | 260 °F | ASTM D1525 |
ExxonMobil Paxon™ BA53-035 Blow Molding Resin
(discontinued **) BA53-035 is a high molecular weight, high density polyethylene copolymer offering an outstanding combination of stiffness and toughness. The resin provides superior melt strength and impact resista.. |
|||
Vicat Softening Point | 127 °C @Load 1.00 kg |
261 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Eraclene® MM 84 U High Density Polyethylene - Injection Molding Eraclene MM 84 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 84 U is characterized by high rigidity and good impac.. |
|||
Vicat Softening Point | 127 °C | 260 °F | ASTM D1525 |
ExxonMobil Paxon™ AU55-003 Blow Molding Resin
(discontinued **) AU55-003 is a blow molding grade high density polyethylene containing an excellent antistat additive, offering a good combination of stiffness and stress crack resistance. An enhanced additive pack.. |