Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 68.0 GPa

@Temperature 482 °C
9860 ksi

@Temperature 900 °F
Cold Worked
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy
MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers..
Shear Modulus 68.0 GPa

@Temperature 600 °C
9860 ksi

@Temperature 1110 °F
Dynamic
Haynes 282® Nickel Alloy Autogenously Welded Sheet
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 68.0 GPa

@Temperature 600 °C
9860 ksi

@Temperature 1110 °F
Dynamic
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 68.0 GPa

@Temperature 600 °C
9860 ksi

@Temperature 1110 °F
Dynamic
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 68.0 GPa

@Temperature 600 °C
9860 ksi

@Temperature 1110 °F
Dynamic
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 68.0 GPa

@Temperature 600 °C
9860 ksi

@Temperature 1110 °F
Dynamic
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 68.0 GPa

@Temperature 600 °C
9860 ksi

@Temperature 1110 °F
Dynamic
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 68.0 GPa

@Temperature 600 °C
9860 ksi

@Temperature 1110 °F
Special Metals INCONEL® alloy N06230 Ni-Cr-W-Mo Alloy
INCONEL® alloy N06230 (UNS N06230 / W.Nr. 2.4733) is a carbide strengthened nickel-chromium-tungsten-molybdenum alloy with an exceptional combination of strength, stability, and resistance to cor..
Shear Modulus 68.0 GPa

@Temperature 600 °C
9860 ksi

@Temperature 1110 °F
Dynamic
Haynes 282® Nickel Alloy Sheet, Gamma-Prime Strengthened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..
Shear Modulus 68.0 GPa

@Temperature 600 °C
9860 ksi

@Temperature 1110 °F
Dynamic
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..