Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.980 GPa @Temperature -20.0 °C |
142 ksi @Temperature -4.00 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |
|||
Shear Modulus | 0.979 GPa @Temperature -50.0 °C |
142 ksi @Temperature -58.0 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |