Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 80.94 GPa @Temperature 25.6 °C |
11740 ksi @Temperature 78.0 °F |
Cold Worked and Aged |
Latrobe MP35N® Alloy MP35N is a nickel-cobalt base alloy of the Multiphase alloy system that has a unique combination of properties - ultra high strength, toughness, ductility, and outstanding corrosion resistance. The .. |