Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 73.0 GPa @Temperature 400 °C |
10600 ksi @Temperature 752 °F |
Dynamic |
Haynes 282® Nickel Alloy Autogenously Welded Sheet Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Shear Modulus | 73.0 GPa @Temperature 400 °C |
10600 ksi @Temperature 752 °F |
Dynamic |
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Shear Modulus | 73.0 GPa @Temperature 400 °C |
10600 ksi @Temperature 752 °F |
Dynamic |
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Shear Modulus | 73.0 GPa @Temperature 400 °C |
10600 ksi @Temperature 752 °F |
Dynamic |
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Shear Modulus | 73.0 GPa @Temperature 400 °C |
10600 ksi @Temperature 752 °F |
Dynamic |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Shear Modulus | 73.0 GPa @Temperature 400 °C |
10600 ksi @Temperature 752 °F |
Dynamic |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Shear Modulus | 73.0 GPa @Temperature 400 °C |
10600 ksi @Temperature 752 °F |
|
Special Metals INCONEL® alloy N06230 Ni-Cr-W-Mo Alloy INCONEL® alloy N06230 (UNS N06230 / W.Nr. 2.4733) is a carbide strengthened nickel-chromium-tungsten-molybdenum alloy with an exceptional combination of strength, stability, and resistance to cor.. |
|||
Shear Modulus | 73.0 GPa @Temperature 400 °C |
10600 ksi @Temperature 752 °F |
Dynamic |
Haynes 282® Nickel Alloy Sheet, Gamma-Prime Strengthened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |
|||
Shear Modulus | 73.0 GPa @Temperature 400 °C |
10600 ksi @Temperature 752 °F |
Dynamic |
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |