Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 70.60 GPa @Temperature 482 °C |
10240 ksi @Temperature 900 °F |
Annealed |
Latrobe MP35N® Alloy MP35N is a nickel-cobalt base alloy of the Multiphase alloy system that has a unique combination of properties - ultra high strength, toughness, ductility, and outstanding corrosion resistance. The .. |