Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 3.90 GPa @Temperature 150 °C |
566 ksi @Temperature 302 °F |
|
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Shear Modulus | 3.90 GPa @Temperature 100 °C |
566 ksi @Temperature 212 °F |
|
Akro-Plastic Akromid® T6 GF 50 (3106) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Shear Modulus | 3.90 GPa @Temperature 232 °C |
566 ksi @Temperature 450 °F |
IM7 (12K); [+/- 45°]2s |
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Tape Form Fiber: T300-12K, IM7-12KInformation provided by HexCel |