Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 2.80 GPa @Temperature 177 °C |
406 ksi @Temperature 351 °F |
IM7 (12K); [+/- 45°]2s; Wet Condition |
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Tape Form Fiber: T300-12K, IM7-12KInformation provided by HexCel |