Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 59.0 MPa @Temperature 23.0 °C |
8560 psi @Temperature 73.4 °F |
DAM; ASTM D732 |
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612
(Unverified Data**) Zytel® 158L NC010 is an intermediate viscosity, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |
|||
Shear Strength | 59.0 MPa @Temperature 23.0 °C |
8560 psi @Temperature 73.4 °F |
ILSS; prEN2563 |
Hexcel® HexPly® M35-4 80-180°C Curing Epoxy Matrix, M35-4/40%/G803/1200 Fabric Fiber: T300 3K, 285 g/m2Information provided by HexCel |