Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 5.45 MPa @Temperature 82.0 °C |
790 psi @Temperature 180 °F |
Overlap, FRP |
3M Scotch-Weld™ TE031 Black Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |