Mechanical Properties Metric English Comments
Shear Strength 29.6 MPa

@Temperature 87.8 °C
4300 psi

@Temperature 190 °F
Short-Beam, Wet (2hr water boil immersion); ASTM D2344
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced
Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f..
Shear Strength 29.6 MPa

@Temperature 98.9 °C
4300 psi

@Temperature 210 °F
Lap Shear
Hexcel® Redux® 312 Modified epoxy film adhesive (0.06 psf)
Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A support..
Shear Strength 29.6 MPa

@Temperature 71.1 °C
4300 psi

@Temperature 160 °F
Lap Shear
Hexcel® Redux® 312/5 Modified epoxy film adhesive
Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A support..
Shear Strength 29.6 MPa

@Temperature 60.0 °C
4300 psi

@Temperature 140 °F
Lap Shear
Hexcel® Redux® 335K Adhesive film for bonding metallic and composite components (0.06 psf)
Redux 335 is a film adhesive curing at 250F. It is available in a range of standard areal weights from 0.015 to 0.06 psf. It is available either unsupported or with knitted and/or matt carrier for a..
Shear Strength 29.6 MPa

@Temperature 60.0 °C
4300 psi

@Temperature 140 °F
Lap Shear
Hexcel® Redux® 335U Adhesive film for bonding metallic and composite components (0.03 psf)
Redux 335 is a film adhesive curing at 250F. It is available in a range of standard areal weights from 0.015 to 0.06 psf. It is available either unsupported or with knitted and/or matt carrier for a..
Shear Strength 29.6 MPa

@Temperature 90.0 °C,
Time 900 sec
4300 psi

@Temperature 194 °F,
Time 0.250 hour
Lap, Alum to Alum
Atom Adhesives AA-BOND F112 Epoxy Adhesive
AA-BOND F112 is an impact resistant, fiber-optic adhesive. AA-BOND F112 is two-part, low viscosity epoxy has the distinct advantage of remaining below 3000 cps for a minimum of 40 minutes. AA-BOND F..