Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 13.77 MPa @Temperature 21.1 °C |
1997 psi @Temperature 70.0 °F |
Lap Shear, Dry; ASTM D1002 |
Renegade Materials Corporation RM-3006 Bismaleimide (BMI) Paste Adhesive Developed using state-of-the-art formulating technologies, RM-3006 BMI Paste Adhesive is a -65°F to 400°F (-54°C to 204°C) service material. RM-3006 was
developed for use with Renegade’s BMI P.. |