Developed using state-of-the-art formulating technologies, RM-3006 BMI Paste Adhesive is a -65°F to 400°F (-54°C to 204°C) service material. RM-3006 was developed for use with Renegade’s BMI Prepregs and Infusion Resins as well as other industry standard BMI systems and metals.Information provided by Renegade Materials Corporation.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
Resin; ASTM D790
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
ASTM D2240
Compressive Strength 0.00758 MPa

@Temperature 177 °C
1.10 psi

@Temperature 350 °F
Dry; ASTM D695
0.159 MPa

@Temperature 21.1 °C
23.0 psi

@Temperature 70.0 °F
Dry; ASTM D695
Shear Strength 6.10 MPa

@Temperature 177 °C
885 psi

@Temperature 350 °F
Lap Shear, Dry; ASTM D1002
13.77 MPa

@Temperature 21.1 °C
1997 psi

@Temperature 70.0 °F
Lap Shear, Dry; ASTM D1002