Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.690 MPa @Temperature 121 °C |
100 psi @Temperature 250 °F |
ASTM D1002-64 |
3M Scotch-Weld™ DP-605NS Off-White Adhesive in Duo-Pak Cartridges
(discontinued **) Features include fast cure adhesive, semi-rigid urethane, 15-20 minutes handling strength, and excellent gap filler and non sag product for wood and plastic. Mix ratio by volume 1:1. Average T-Peel.. |
|||
Shear Strength | 0.689 MPa @Temperature 82.0 °C |
100 psi @Temperature 180 °F |
Overlap, Solvent Wiped Al |
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 0.689 MPa @Temperature 82.0 °C |
100 psi @Temperature 180 °F |
Overlap, Abraded and Solvent Wiped Steel |
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 0.689 MPa @Temperature 82.0 °C |
100 psi @Temperature 180 °F |
Overlap, Solvent Wiped Al |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 0.689 MPa @Temperature 82.0 °C |
100 psi @Temperature 180 °F |
Overlap, Abraded and Solvent Wiped Steel |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 0.689 MPa @Temperature 82.0 °C |
100 psi @Temperature 180 °F |
Overlap, Solvent Wiped Al |
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 0.689 MPa @Temperature 82.0 °C |
100 psi @Temperature 180 °F |
Overlap, Abraded and Solvent Wiped Steel |
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |