Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 78.5 MPa @Temperature 150 °C |
11400 psi @Temperature 302 °F |
JIS K7214 |
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |