Mechanical Properties Metric English Comments
Shear Strength 46.9 MPa

@Temperature 177 °C
6800 psi

@Temperature 350 °F
Inter-laminar, Wet; SACMA SRM 7R-94
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric
MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties ..
Shear Strength 46.9 MPa

@Temperature 21.1 °C
6800 psi

@Temperature 70.0 °F
Lap Shear
Hexcel® Redux® 308 Modified epoxy film adhesive
Redux 308 is a high-strength film adhesive curing at 350°F. It is suitable for a wide range of structural bonding applications including metal to metal bonding and sandwich constructions, where ope..
Shear Strength 46.9 MPa

@Temperature 21.1 °C
6800 psi

@Temperature 70.0 °F
Lap Shear
Hexcel® Redux® 335U Adhesive film for bonding metallic and composite components (0.06 psf)
Redux 335 is a film adhesive curing at 250F. It is available in a range of standard areal weights from 0.015 to 0.06 psf. It is available either unsupported or with knitted and/or matt carrier for a..