Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 27.6 MPa @Temperature 21.1 °C |
4010 psi @Temperature 70.0 °F |
Cure Cycle, 6 hrs @ 200°F, FPL Acid Etched 6061-T6, Std Dev 109; ASTM D1002 |
Zyvex Performance Materials Aroply™ 250 Nano-Engineered Composite Film Adhesive Aroply™ 250 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported knitted nylon carrier. Cured adhe.. |
|||
Shear Strength | 27.6 MPa @Temperature 23.9 °C |
4000 psi @Temperature 75.0 °F |
Cure cycle: 12 hrs @ RT + 1 hr @ 176°F, with Aced Etched 6061-T6 Aluminum |
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Liquid Epovex® Adhesive is a carbon nanotube enhanced ambient or elevated temperature cure two-part epoxy adhesive. Used for bonding, laminating, filling or potting, Epovex is ideal for many metals, woods.. |
|||
Shear Strength | 27.6 MPa @Temperature 23.9 °C |
4000 psi @Temperature 75.0 °F |
Cure cycle: 7 days @ RT, with Aced Etched 6061-T6 Aluminum |
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Paste Epovex® Adhesive Paste is a carbon nanotube enhanced two part epoxy adhesive thixotropic paste. Used for bonding or filling, Epovex Paste is ideal for many metals, woods, masonry products, and some.. |
|||
Shear Strength | 27.6 MPa @Temperature 23.9 °C |
4000 psi @Temperature 75.0 °F |
Cure cycle: 12 hrs @ RT + 1 hr @ 176°F, with Aced Etched 6061-T6 Aluminum |
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Paste Epovex® Adhesive Paste is a carbon nanotube enhanced two part epoxy adhesive thixotropic paste. Used for bonding or filling, Epovex Paste is ideal for many metals, woods, masonry products, and some.. |
|||
Shear Strength | 27.6 MPa @Temperature 204 °C |
4000 psi @Temperature 400 °F |
Tensile Lap Shear; Aluminum Primer HP655P; ASTM D1002 |
Hexcel® Redux® HP655 Toughened BMI film Adhesive Redux® HP655 is a toughened BMI structural adhesive designed for metal to metal, composite to composite, and honeycomb sandwich bonding for both co-cured and precured composite skins. Redux® HP655.. |
|||
Shear Strength | 27.6 MPa @Temperature 204 °C |
4000 psi @Temperature 400 °F |
Tensile Lap Shear; Titanium with HP655P; ASTM D1002 |
Hexcel® Redux® HP655 Toughened BMI film Adhesive Redux® HP655 is a toughened BMI structural adhesive designed for metal to metal, composite to composite, and honeycomb sandwich bonding for both co-cured and precured composite skins. Redux® HP655.. |
|||
Shear Strength | 27.6 MPa @Temperature 24.0 °C |
4000 psi @Temperature 75.2 °F |
Aluminum Overlap |
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive 3M™ Scotch-Weld™ Non-Metallic Filled is a non-metal filled version of Scotch-Weld adhesive 2214 regular. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a pa.. |