Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 117 MPa @Temperature 25.0 °C |
17000 psi @Temperature 77.0 °F |
In-Plane +/- 45 tensile shear; Dry |
Hexcel® HexPly® 8551-7 Epoxy Matrix, IM7 Fiber Information provided by HexCel |
|||
Shear Strength | 117 MPa @Temperature 25.0 °C |
16900 psi @Temperature 77.0 °F |
0° Short Beam, Wet |
Hexcel® HexPly® 8552 Epoxy Matrix, AS4 Fiber Information provided by HexCel |