Polymer Property : Shear Strength = 115 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 115 MPa

@Temperature 23.9 °C
16700 psi

@Temperature 75.0 °F
Short Beam; Dry; ASTM D2344
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 7781 E-Glass Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..
Shear Strength 115 MPa

@Temperature 25.0 °C
16700 psi

@Temperature 77.0 °F
0° Short Beam, Wet
Hexcel® HexPly® 8552 Epoxy Matrix, IM7 Fiber
Information provided by HexCel